GILDING OF SMALL PARTS IN THE MORTAR
|
|
 |
The charge:
The minimum charge to the smallest mortar amounts to approx. 10 g. |
 |
The parameters of the coat:
Thickness of the coat - 0,05-10 µm, on the nickel subcoat or without subcoat
("hard" gold - the addition of nickel). |
 |
Requirements:
Parts to be gilded have to be made of copper, brass, nickel, argentan, bronze, steel, or silver. The parts can not get stuck together during the gilding in the mortar.
|